Calophyllaceae
The family Calophyllaceae supplies 5 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
1 of 5 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Alexandrian laurelCalophyllum inophyllum | 1,255 lbf* | 43.0 lb/ft³ |
| Mammee appleMammea americana | 1,852 lbf* | 51.5 lb/ft³ |
| ManapauMammea glauca | 2,867 lbf* | 63.1 lb/ft³ |
| OlebtachesCalophyllum soulattri | 1,054 lbf* | 39.6 lb/ft³ |
| Santa MariaCalophyllum brasiliense | 1,150 lbf | 39.0 lb/ft³ |