Wood Record

family

Cannabaceae

The family Cannabaceae supplies 7 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

1 of 7 carry a published Janka test.

WoodJankaDensity
Celtis paniculataCeltis paniculata1,309 lbf*43.8 lb/ft³
Chinese hackberryCeltis sinensis915 lbf*37.1 lb/ft³
HackberryCeltis occidentalis880 lbf37.1 lb/ft³
Lamarck's tremaTrema lamarckiana479 lbf*27.5 lb/ft³
MageleTrema cannabina451 lbf*26.7 lb/ft³
Oriental tremaTrema orientalis451 lbf*26.7 lb/ft³
SugarberryCeltis laevigata915 lbf*37.1 lb/ft³