The family Capparaceae supplies 3 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
0 of 3 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| LinguamCapparis indica | 1,923 lbf* | 52.4 lb/ft³ |
| RatappleMorisonia americana | 2,607 lbf* | 60.4 lb/ft³ |
| Sacred garlic pearCrateva religiosa | 753 lbf* | 33.9 lb/ft³ |