Wood Record

family

Caryocaraceae

The family Caryocaraceae supplies 3 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

3 of 3 carry a published Janka test.

WoodJankaDensity
PequiáCaryocar villosum1,133 lbf48.7 lb/ft³
PequiaranaCaryocar glabrum1,642 lbf48.7 lb/ft³
PiquiaCaryocar spp.1,720 lbf54.0 lb/ft³