Wood Record

family

Casuarinaceae

The family Casuarinaceae supplies 3 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

0 of 3 carry a published Janka test.

WoodJankaDensity
Beach sheoakCasuarina equisetifolia3,241 lbf*66.9 lb/ft³
Gray sheoakCasuarina glauca2,448 lbf*58.7 lb/ft³
River sheoakCasuarina cunninghamiana1,990 lbf*53.3 lb/ft³