family
Celastraceae
The family Celastraceae supplies 6 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
1 of 6 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Carne D'AntaMaytenus spp. | 2,240 lbf | 54.0 lb/ft³ |
| Florida boxwoodSchaefferia frutescens | 1,852 lbf* | 51.5 lb/ft³ |
| MaidenberryCrossopetalum rhacoma | 2,963 lbf* | 64.1 lb/ft³ |
| MaytenMaytenus boaria | 1,538 lbf* | 47.3 lb/ft³ |
| PerupokLophopetalum spp. | 791 lbf* | 35.0 lb/ft³ |
| West Indian false boxGyminda latifolia | 2,867 lbf* | 63.1 lb/ft³ |