The family Chrysobalanaceae supplies 13 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

8 of 13 carry a published Janka test.

WoodJankaDensity
Anoerá-ferroAcioa sp2,683 lbf60.6 lb/ft³
Bkau, apgauMaranthes corymbosa2,963 lbf*64.1 lb/ft³
BuradaParinari spp.1,830 lbf52.0 lb/ft³
CaraipéLicania octandra2,754 lbf61.3 lb/ft³
CaraiperanaLicania gracilipes3,294 lbf63.7 lb/ft³
Castanha-de-cutiaCouepia robusta3,206 lbf64.3 lb/ft³
Castanha-de-cutiaAcioa edulis2,696 lbf64.9 lb/ft³
Icaco coco plumChrysobalanus icaco2,210 lbf*55.9 lb/ft³
Macucu-brancoLicania oblongifolia3,153 lbf58.7 lb/ft³
Parinari / bafo-de-boi-mirimParinari excelsa2,522 lbf57.4 lb/ft³
PigeonberryHirtella triandra1,990 lbf*53.3 lb/ft³
SeaParinari insularum1,852 lbf*51.5 lb/ft³