Wood Record

family

Clusiaceae

The family Clusiaceae supplies 9 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

0 of 9 carry a published Janka test.

WoodJankaDensity
Butter treePentadesma butyracea2,530 lbf*59.6 lb/ft³
CupeilloClusia clusioides2,210 lbf*55.9 lb/ft³
Cupey de monteClusia minor509 lbf*28.2 lb/ft³
GarciniaGarcinia myrtifolia2,367 lbf*57.7 lb/ft³
Garcinia xanthochymusGarcinia xanthochymus2,530 lbf*59.6 lb/ft³
GourkaGarcinia dulcis2,210 lbf*55.9 lb/ft³
MangosteenGarcinia mangostana2,530 lbf*59.6 lb/ft³
Palo de cruzGarcinia portoricensis2,779 lbf*62.2 lb/ft³
Scotch attorneyClusia rosea1,538 lbf*47.3 lb/ft³