Wood Record

family

Combretaceae

The family Combretaceae supplies 24 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

13 of 24 carry a published Janka test.

WoodJankaDensity
Bakauaine, nanaLumnitzera littorea1,923 lbf*52.4 lb/ft³
Buttonwood-mangroveConocarpus erectus2,692 lbf*61.3 lb/ft³
Cachaporra-do-gentioTerminalia cf argentea3,139 lbf60.6 lb/ft³
CuiaranaBuchenavia grandis2,513 lbf55.6 lb/ft³
East Indian almondTerminalia myriocarpa1,152 lbf*41.3 lb/ft³
IdígboTerminalia ivorensis845 lbf32.0 lb/ft³
Indian Almond WoodTerminalia catappa1,030 lbf*40.0 lb/ft³
Indian LaurelTerminalia tomentosa complex2,220 lbf54.0 lb/ft³
JucaroBucida bucaras4,305 lbf*69.0 lb/ft³
LimbaTerminalia superba490 lbf34.0 lb/ft³
MaliliTerminalia richii1,309 lbf*43.8 lb/ft³
NargustaTermi nalia amazonia1,855 lbf50.0 lb/ft³
Peruvian almondTerminalia oblonga1,788 lbf*50.7 lb/ft³
Strand treeTerminalia litoralis1,203 lbf*42.1 lb/ft³
TalieTerminalia samoensis1,538 lbf*47.3 lb/ft³
TanibocaBuchenavia cf viridiflora2,191 lbf54.9 lb/ft³
TanimbucaBuchenavia sp2,829 lbf53.7 lb/ft³
TanimbucaBuchenavia tetraphylla = Buchenavia capitata1,640 lbf52.4 lb/ft³
TanimbucaTerminalia amazonia2,235 lbf64.1 lb/ft³
Tropical almondTerminalia kaernbachii1,152 lbf*41.3 lb/ft³
White BombayTerminalia procera1,070 lbf40.0 lb/ft³
White ChuglamTerminalia bialata1,190 lbf43.0 lb/ft³
White mangroveLaguncularia racemosa1,363 lbf*44.7 lb/ft³
Yellow SandersBuchenavia capitata1,220 lbf47.0 lb/ft³