Wood Record

family

Dilleniaceae

The family Dilleniaceae supplies 3 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

1 of 3 carry a published Janka test.

WoodJankaDensity
ChultaDillenia indica1,255 lbf*43.0 lb/ft³
Shrubby dilleniaDillenia suffruticosa1,203 lbf*42.1 lb/ft³
SimpohDillenia spp.1,250 lbf45.0 lb/ft³