Wood Record

family

Ebenaceae

The family Ebenaceae supplies 9 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

2 of 9 carry a published Janka test.

WoodJankaDensity
African ebonyDiospyros spp.3,220 lbf63.0 lb/ft³
AuauliDiospyros samoensis1,725 lbf*49.9 lb/ft³
Common persimmonDiospyros virginiana1,725 lbf*49.9 lb/ft³
Diospyros ferreaDiospyros ferrea2,692 lbf*61.3 lb/ft³
East Indian ebonyDiospyros spp.1,630 lbf52.0 lb/ft³
LamaDiospyros sandwicensis2,607 lbf*60.4 lb/ft³
MaboloDiospyros discolor3,147 lbf*65.9 lb/ft³
PersimmonDiospyros kaki1,725 lbf*49.9 lb/ft³
Texas persimmonDiospyros texana1,725 lbf*49.9 lb/ft³