Wood Record

family

Ericaceae

The family Ericaceae supplies 6 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

0 of 6 carry a published Janka test.

WoodJankaDensity
Arizona madroneArbutus arizonica1,363 lbf*44.7 lb/ft³
FarkleberryVaccinium arboreum1,658 lbf*48.9 lb/ft³
Pacific madroneArbutus menziesii1,363 lbf*44.7 lb/ft³
SourwoodOxydendrum arboreum960 lbf*38.0 lb/ft³
Strawberry treeArbutus unedo1,363 lbf*44.7 lb/ft³
Texas madroneArbutus xalapensis1,363 lbf*44.7 lb/ft³