family
Euphorbiaceae
The family Euphorbiaceae supplies 40 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
12 of 40 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AchiotilloAlchornea latifolia | 753 lbf* | 33.9 lb/ft³ |
| AlomMelanolepis multiglandulosa | 479 lbf* | 27.5 lb/ft³ |
| Barbados nutJatropha curcas | 181 lbf* | 17.5 lb/ft³ |
| BishopwoodBischofia javanica | 1,370 lbf | 44.0 lb/ft³ |
| Blinding treeExcoecaria agallocha | 641 lbf* | 31.5 lb/ft³ |
| Burra-leiteiraSapium marmieri | 324 lbf | 30.0 lb/ft³ |
| Castanha-de-araraJoannesia heveoides | 582 lbf | 29.1 lb/ft³ |
| CastorbeanRicinus communis | 395 lbf* | 25.1 lb/ft³ |
| CauchoranaMicrandra minor | 703 lbf | 30.0 lb/ft³ |
| Chinese tallowTriadica sebifera | 542 lbf* | 29.1 lb/ft³ |
| ErimadoRicinodendron heudelotii | 121 lbf* | 15.0 lb/ft³ |
| FanuamamalaHomalanthus nutans | 608 lbf* | 30.7 lb/ft³ |
| Garden crotonCodiaeum variegatum | 1,007 lbf* | 38.8 lb/ft³ |
| GlíciaGlycydendron amazonicum | 1,671 lbf | 51.5 lb/ft³ |
| GubasEndospermum spp. | 509 lbf* | 30.0 lb/ft³ |
| HinchahuevosSapium laurifolium | 542 lbf* | 29.1 lb/ft³ |
| HuraHura crepitans | 550 lbf | 30.0 lb/ft³ |
| Indian spurgetreeEuphorbia neriifolia | 451 lbf* | 26.7 lb/ft³ |
| Indiantree spurgeEuphorbia tirucalli | 542 lbf* | 29.1 lb/ft³ |
| Kamala treeMallotus philippensis | 1,363 lbf* | 44.7 lb/ft³ |
| LecheroSapium spp. | 700 lbf | 36.0 lb/ft³ |
| LeiteiroSapium glandulosum = Sapium aereum | 379 lbf | 32.5 lb/ft³ |
| ManchineelHippomane mancinella | 960 lbf* | 38.0 lb/ft³ |
| MilktreeSapium laurocerasus | 509 lbf* | 28.2 lb/ft³ |
| Mu oil treeVernicia montana | 423 lbf* | 26.0 lb/ft³ |
| MusineCroton megalocarpus | 1,350 lbf | 44.0 lb/ft³ |
| OysterwoodGymnanthes lucida | 3,965 lbf* | 73.4 lb/ft³ |
| Palo de gallinaAlchorneopsis floribunda | 608 lbf* | 30.7 lb/ft³ |
| Parasol leaf treeMacaranga tanarius | 479 lbf* | 27.5 lb/ft³ |
| Pau-brancoDrypetes variabilis | 2,518 lbf | 55.9 lb/ft³ |
| PenguaMacaranga mappa | 423 lbf* | 26.0 lb/ft³ |
| PoinsettiaEuphorbia pulcherrima | 714 lbf* | 33.1 lb/ft³ |
| RubberwoodHevea brasiliensis | 915 lbf* | 38.0 lb/ft³ |
| SabinonCroton poecilanthus | 1,203 lbf* | 42.1 lb/ft³ |
| SeringaranaMicrandra rossiana | 1,925 lbf | 50.6 lb/ft³ |
| Shirakiopsis indicaShirakiopsis indica | 915 lbf* | 37.1 lb/ft³ |
| Sugar-PlumUapaca spp. | 1,447 lbf* | 46.0 lb/ft³ |
| SuradanHyeronima alchorneoides | 1,700 lbf | 50.0 lb/ft³ |
| TreadsoftlyCnidoscolus aconitifolius | 197 lbf* | 18.2 lb/ft³ |
| Tungoil treeVernicia fordii | 479 lbf* | 27.5 lb/ft³ |