Wood Record

family

Flacourtiaceae

The family Flacourtiaceae supplies 6 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

5 of 6 carry a published Janka test.

WoodJankaDensity
African HomaliumHomalium spp.2,050 lbf54.0 lb/ft³
Burma LancewoodHomalium spp.2,270 lbf58.0 lb/ft³
MuirungiCasearia battiscombei720 lbf40.0 lb/ft³
OdokoScottellia coriacea1,090 lbf41.0 lb/ft³
Pau-jacaréLaetia procera2,053 lbf52.4 lb/ft³
West Indian BoxwoodGossypiospermum praecox2,064 lbf*53.0 lb/ft³