The family Guttiferae supplies 8 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

4 of 8 carry a published Janka test.

WoodJankaDensity
BintangorCalophyllum spp.1,475 lbf40.0 lb/ft³
CamaçariCaraipa densifolia1,515 lbf48.7 lb/ft³
GangawMesua ferrea2,890 lbf63.0 lb/ft³
GeronggangCratoxylon arborescens573 lbf*30.0 lb/ft³
KandisGarcinia spp.2,530 lbf*58.0 lb/ft³
ManniSymphonia globulifera1,120 lbf44.0 lb/ft³
ObotoMammea africana1,568 lbf*48.0 lb/ft³
PacuriRheedia spp.2,287 lbf*55.0 lb/ft³