Juglandaceae
The family Juglandaceae supplies 22 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
7 of 22 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Arizona walnutJuglans major | 714 lbf* | 33.1 lb/ft³ |
| Bitternut hickoryCarya cordiformis | 1,461 lbf* | 46.1 lb/ft³ |
| Black hickoryCarya texana | 1,598 lbf* | 48.1 lb/ft³ |
| Black walnutJuglans nigra | 1,010 lbf | 38.5 lb/ft³ |
| ButternutJuglans cinerea | 490 lbf | 26.6 lb/ft³ |
| Chinese wingnutPterocarya stenoptera | 451 lbf* | 26.7 lb/ft³ |
| English walnutJuglans regia | 714 lbf* | 33.1 lb/ft³ |
| Mockernut hickoryCarya alba | 1,970 lbf | 50.3 lb/ft³ |
| NogalJuglans spp. | 960 lbf* | 38.0 lb/ft³ |
| Northern California black walnutJuglans hindsii | 714 lbf* | 33.1 lb/ft³ |
| Nutmeg hickoryCarya myristiciformis | 1,190 lbf* | 42.0 lb/ft³ |
| Pecan hickoryCarya illinoinensis | 1,820 lbf | 46.1 lb/ft³ |
| Pignut hickoryCarya glabra | 2,140 lbf | 52.4 lb/ft³ |
| Red hickoryCarya ovalis | 1,598 lbf* | 48.1 lb/ft³ |
| Sand hickoryCarya pallida | 1,598 lbf* | 48.1 lb/ft³ |
| Scrub hickoryCarya floridana | 1,598 lbf* | 48.1 lb/ft³ |
| Shagbark hickoryCarya ovata | 1,880 lbf | 50.3 lb/ft³ |
| Shellbark hickoryCarya laciniosa | 1,810 lbf | 48.3 lb/ft³ |
| Southern California black walnutJuglans californica | 714 lbf* | 33.1 lb/ft³ |
| Southern shagbark hickoryCarya carolinae-septentrionalis | 1,598 lbf* | 48.1 lb/ft³ |
| Texas walnutJuglans microcarpa | 714 lbf* | 33.1 lb/ft³ |
| Water hickoryCarya aquatica | 1,277 lbf* | 43.3 lb/ft³ |