The family Lamiaceae supplies 12 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
0 of 12 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AloaloPremna serratifolia | 1,007 lbf* | 38.8 lb/ft³ |
| AzulejoCornutia pyramidata | 2,064 lbf* | 54.2 lb/ft³ |
| BarsVitex cofassus | 1,725 lbf* | 49.9 lb/ft³ |
| Bastard stopperPetitia domingensis | 1,658 lbf* | 48.9 lb/ft³ |
| BelauGmelina elliptica | 875 lbf* | 36.3 lb/ft³ |
| BlacheosGmelina palawensis | 960 lbf* | 38.0 lb/ft³ |
| Chinese chastetreeVitex negundo | 1,054 lbf* | 39.6 lb/ft³ |
| HiguerilloVitex divaricata | 1,309 lbf* | 43.8 lb/ft³ |
| Lilac chastetreeVitex agnus-castus | 1,363 lbf* | 44.7 lb/ft³ |
| Simpleleaf chastetreeVitex trifolia | 1,309 lbf* | 43.8 lb/ft³ |
| Smallflower chastetreeVitex parviflora | 2,139 lbf* | 55.1 lb/ft³ |
| StickbushClerodendrum chinense | 509 lbf* | 28.2 lb/ft³ |