WoodJankaDensity
AlbarcoCariniana spp.1,020 lbf35.0 lb/ft³
Cannonball treeCouroupita guianensis714 lbf*33.1 lb/ft³
CastanheiraBertholletia excelsa1,470 lbf48.9 lb/ft³
EssiaCombretodendron macrocarpum2,180 lbf53.0 lb/ft³
JaranaHolopyxidium jarana3,500 lbf62.0 lb/ft³
LangaasagBarringtonia racemosa753 lbf*33.9 lb/ft³
MahotCouratari spp.960 lbf*37.0 lb/ft³
ManbarklakEschweilera spp.3,480 lbf46.2 lb/ft³
MatamatáEschweilera coriacea2,467 lbf56.2 lb/ft³
MatamatáEschweilera grandiflora = Eschweilera cf fracta1,995 lbf53.1 lb/ft³
MatamatáEschweilera pedicellata = Eschweilera longipes2,410 lbf61.2 lb/ft³
Matamatá / sapucaia-amargosaLecythis idatimon2,341 lbf60.4 lb/ft³
Putat PayaPlanchonia spp.1,355 lbf48.0 lb/ft³
SapucaiaLecythis spp.3,100 lbf58.0 lb/ft³
Sapucaia / sapucaia-vermelhaLecythis pisonis subsp. usitata2,831 lbf67.7 lb/ft³
Sea putatBarringtonia asiatica608 lbf*30.7 lb/ft³
SeruAllantoma lineata1,153 lbf46.8 lb/ft³
TauariCouratari oblongifolia936 lbf37.5 lb/ft³
TauariCouratari guianensis1,138 lbf39.6 lb/ft³
TauariCouratari stellata1,565 lbf50.7 lb/ft³