family
Lythraceae
The family Lythraceae supplies 6 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
1 of 6 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| CrapemyrtleLagerstroemia indica | 1,419 lbf* | 45.5 lb/ft³ |
| MangroveSonneratia alba | 1,309 lbf* | 43.8 lb/ft³ |
| NgisPemphis acidula | 4,305 lbf* | 76.3 lb/ft³ |
| PomegranatePunica granatum | 1,990 lbf* | 53.3 lb/ft³ |
| Pride of IndiaLagerstroemia speciosa | 1,203 lbf* | 42.1 lb/ft³ |
| PyinmaLagerstroemia spp. | 1,055 lbf | 43.0 lb/ft³ |