family
Magnoliaceae
The family Magnoliaceae supplies 14 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
5 of 14 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Bigleaf magnoliaMagnolia macrophylla | 679 lbf* | 32.3 lb/ft³ |
| ChampacaMichelia spp. | 725 lbf | 31.0 lb/ft³ |
| CucumbertreeMagnolia acuminata | 700 lbf | 33.6 lb/ft³ |
| Fraser magnoliaMagnolia fraseri | 573 lbf* | 29.8 lb/ft³ |
| Laurel magnoliaMagnolia splendens | 1,203 lbf* | 42.1 lb/ft³ |
| MagnoliaMagnolia spp. | 1,090 lbf | 39.0 lb/ft³ |
| Oyama magnoliaMagnolia sieboldii | 679 lbf* | 32.3 lb/ft³ |
| Puerto Rico magnoliaMagnolia portoricensis | 1,203 lbf* | 42.1 lb/ft³ |
| Pyramid magnoliaMagnolia pyramidata | 679 lbf* | 32.3 lb/ft³ |
| Southern magnoliaMagnolia grandiflora | 1,020 lbf | 35.0 lb/ft³ |
| Star magnoliaMagnolia stellata | 679 lbf* | 32.3 lb/ft³ |
| Sweetbay magnoliaMagnolia virginiana | 875 lbf* | 36.3 lb/ft³ |
| Umbrella magnoliaMagnolia tripetala | 679 lbf* | 32.3 lb/ft³ |
| Yellow-poplarLiriodendron tulipifera | 540 lbf | 29.3 lb/ft³ |