The family Malpighiaceae supplies 6 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
0 of 6 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Cafe forasteroBunchosia glandulosa | 1,990 lbf* | 53.3 lb/ft³ |
| DoncellaByrsonima spicata | 1,419 lbf* | 45.5 lb/ft³ |
| Long Key locustberryByrsonima lucida | 1,203 lbf* | 42.1 lb/ft³ |
| Maricao cimunByrsonima crassifolia | 1,475 lbf* | 46.4 lb/ft³ |
| SerretteByrsonima coriacea var. spicata | 1,538 lbf* | 46.0 lb/ft³ |
| Wild crapemyrtleMalpighia glabra | 2,064 lbf* | 54.2 lb/ft³ |