Wood Record

family

Malvaceae

The family Malvaceae supplies 30 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

1 of 30 carry a published Janka test.

WoodJankaDensity
Abata colaCola acuminata1,419 lbf*45.5 lb/ft³
American basswoodTilia americana410 lbf25.8 lb/ft³
BaobabAdansonia digitata321 lbf*22.8 lb/ft³
BastardcedarGuazuma ulmifolia1,007 lbf*38.8 lb/ft³
CacaoTheobroma cacao641 lbf*31.5 lb/ft³
Chinese parasoltreeFirmiana simplex641 lbf*31.5 lb/ft³
ChuchabColona scabra509 lbf*28.2 lb/ft³
DurianDurio zibethinus915 lbf*37.1 lb/ft³
Guest treeKleinhovia hospita641 lbf*31.5 lb/ft³
Hazel sterculiaSterculia foetida875 lbf*36.3 lb/ft³
Hierba del soldadoMelochia umbellata451 lbf*26.7 lb/ft³
Largeleaf rosemallowHibiscus macrophyllus641 lbf*31.5 lb/ft³
Littleleaf lindenTilia cordata344 lbf*23.5 lb/ft³
LueheaLuehea speciosa1,363 lbf*44.7 lb/ft³
MagaThespesia grandiflora1,475 lbf*46.4 lb/ft³
MahoeHibiscus elatus1,007 lbf*38.8 lb/ft³
MaoCommersonia bartramia542 lbf*29.1 lb/ft³
MaouliTrichospermum richii395 lbf*25.1 lb/ft³
Miich era ngebard, guiana chestnutPachira aquatica753 lbf*33.9 lb/ft³
Pink flame treeBrachychiton discolor216 lbf*19.0 lb/ft³
PochoteCeiba aesculifolia641 lbf*31.5 lb/ft³
Portia treeThespesia populnea1,103 lbf*40.5 lb/ft³
ShoeblackplantHibiscus rosa-sinensis451 lbf*26.7 lb/ft³
Silver lindenTilia tomentosa344 lbf*23.5 lb/ft³
Swizzlestick treeQuararibea turbinata1,309 lbf*43.8 lb/ft³
TeabushMelochia tomentosa2,064 lbf*54.2 lb/ft³
Trichospermum ikutaiTrichospermum ikutai423 lbf*26.0 lb/ft³
UfaHeritiera littoralis2,367 lbf*57.7 lb/ft³
Wild chestnutPachira insignis714 lbf*33.1 lb/ft³
Yellow llimaSida fallax1,538 lbf*47.3 lb/ft³