Wood Record

family

Melastomataceae

The family Melastomataceae supplies 13 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

2 of 13 carry a published Janka test.

WoodJankaDensity
AuqueyMiconia punctata1,419 lbf*45.5 lb/ft³
Camasey cuatrocanalesMiconia mirabilis1,203 lbf*42.1 lb/ft³
Camasey de costillaMiconia impetiolaris1,598 lbf*48.1 lb/ft³
Camasey felpaMiconia racemosa1,054 lbf*39.6 lb/ft³
Camasey peludoHenriettea fascicularis1,309 lbf*43.8 lb/ft³
Granadillo boboMiconia prasina1,363 lbf*44.7 lb/ft³
Jau jauMiconia serrulata1,309 lbf*43.8 lb/ft³
JongkongDactylocladus stenostachys720 lbf34.0 lb/ft³
Melastoma sanguineumMelastoma sanguineum1,007 lbf*38.8 lb/ft³
MiraúbaMouriri collocarpa4,032 lbf68.0 lb/ft³
RajadorMiconia tetrandra1,852 lbf*51.5 lb/ft³
SaquiyacMiconia affinis1,475 lbf*46.4 lb/ft³
Velvet treeMiconia calvescens1,103 lbf*40.5 lb/ft³