The family Meliaceae supplies 34 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

18 of 34 carry a published Janka test.

WoodJankaDensity
African mahoganyKhaya spp.830 lbf32.0 lb/ft³
African-WalnutLovoa trichilioides syn. L klaineana940 lbf34.0 lb/ft³
AlligatorwoodGuarea glabra1,309 lbf*43.8 lb/ft³
American muskwoodGuarea guidonia1,363 lbf*44.7 lb/ft³
AmooraAmoora spp.895 lbf46.0 lb/ft³
AndirobaCarapa guianensis1,130 lbf41.0 lb/ft³
Australian redcedarToona ciliata641 lbf*31.5 lb/ft³
AvodireTurraeanthus africanus1,080 lbf36.0 lb/ft³
BroomstickTrichilia hirta1,598 lbf*48.1 lb/ft³
CangeranaCab ralea can ge rana1,203 lbf*42.0 lb/ft³
CedroCedrela odorata1,373 lbf29.3 lb/ft³
ChickrassyChukrasia tabularis1,310 lbf42.0 lb/ft³
CramanteeGuarea spp.1,065 lbf39.0 lb/ft³
Dysoxylum mollissimum ssp. MolleDysoxylum mollissimum1,152 lbf*41.3 lb/ft³
EkebergiaEkebergia rueppelliana900 lbf38.0 lb/ft³
GaitaTrichilia pallida1,363 lbf*44.7 lb/ft³
Gedu NohorEntandrophragma angolense940 lbf34.0 lb/ft³
GuareaGuarea cedrata1,000 lbf36.0 lb/ft³
Khaya anthothecaKhaya anthotheca960 lbf*38.0 lb/ft³
KosipoEntandrophragma candollei1,391 lbf*45.0 lb/ft³
LalanyogXylocarpus granatum1,309 lbf*43.8 lb/ft³
LeileiXylocarpus moluccensis1,475 lbf*46.4 lb/ft³
NeemAzadirachta spp.1,460 lbf40.0 lb/ft³
NeemAzadirachta indica1,852 lbf*51.5 lb/ft³
Persian LilacMelia azedarach832 lbf*36.0 lb/ft³
Pracuúba-da-terra-firmeTrichilia lecointei3,159 lbf73.4 lb/ft³
Santol, kechapiSandoricum koetjape714 lbf*33.1 lb/ft³
SapeleEntandrophragma cylindricum1,510 lbf42.0 lb/ft³
Senegal mahoganyKhaya senegalensis1,725 lbf*49.9 lb/ft³
Spanish-cedarCedrela spp.600 lbf35.0 lb/ft³
ToonCedrela spp. (mainly C toona)550 lbf31.5 lb/ft³
True mahoganySwietenia macrophylla800 lbf41.0 lb/ft³
UtileEntandrophragma utile1,260 lbf41.0 lb/ft³
West Indian mahoganySwietenia mahagoni1,419 lbf*45.5 lb/ft³