family
Mimosaceae
The family Mimosaceae supplies 17 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
17 of 17 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Angelim / angelim-rajadoZygia racemosa = Marmaroxylon racemosum | 3,177 lbf | 61.8 lb/ft³ |
| Angelim-vermelhoDinizia excelsa | 3,045 lbf | 66.9 lb/ft³ |
| AngicoPeltogyne cf subsessilis | 2,941 lbf | 60.6 lb/ft³ |
| Fava-bolota / visgueiroParkia gigantocarpa | 463 lbf | 19.4 lb/ft³ |
| Fava-orelha-de-negroEnterolobium schomburgkii | 2,346 lbf | 62.0 lb/ft³ |
| FaveiraParkia nitida = Parkia oppositifolia | 621 lbf | 27.5 lb/ft³ |
| FaveiraParkia multijuga | 668 lbf | 28.2 lb/ft³ |
| Faveira / visgueiroParkia paraensis | 743 lbf | 33.1 lb/ft³ |
| IngáInga paraensis | 3,064 lbf | 65.9 lb/ft³ |
| IngáInga sp | 2,846 lbf | 68.7 lb/ft³ |
| Ingá / ingá xixiInga alba | 1,418 lbf | 48.1 lb/ft³ |
| Inga-de-porcoAlbizia pedicellaris = Macrosamanea pedicellaris | 955 lbf | 38.1 lb/ft³ |
| MonjoleiroSenegalia polyphylla = Acacia polyphylla | 1,093 lbf | 46.2 lb/ft³ |
| TamborilEnterolobium maximum | 691 lbf | 29.5 lb/ft³ |
| TimboranaPseudopiptadenia suaveolens =Piptadenia suaveolens | 1,537 lbf | 34.3 lb/ft³ |
| TornilloCedrelinga cateniformis | 787 lbf | 35.0 lb/ft³ |
| XixáSterculia excelsa = Sterculia speciosa | 1,071 lbf | 39.4 lb/ft³ |