The family Myristicaceae supplies 12 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

10 of 12 carry a published Janka test.

WoodJankaDensity
CuangareDialyanthera spp.380 lbf28.0 lb/ft³
Darah DarahMyristica spp.1,020 lbf40.0 lb/ft³
IlombaPycnanthus angolensis610 lbf29.8 lb/ft³
KirikawaIryanthera spp.930 lbf35.0 lb/ft³
MtambaraCephalosphaera usambarensis740 lbf37.0 lb/ft³
NiovéStaudtia stipitata2,530 lbf*57.0 lb/ft³
SorroScyphocephalium ochocoa875 lbf*36.0 lb/ft³
Ucuúba / virolaVirola multicostata496 lbf35.5 lb/ft³
UcuubaranaOsteophloeum platyspermum817 lbf36.8 lb/ft³
UcuubaranaIryanthera grandis1,195 lbf48.9 lb/ft³
VirolaVirola michelii1,041 lbf38.0 lb/ft³
Virola / ucuúba-cheirosaVirola surinamensis624 lbf28.7 lb/ft³