Wood Record

family

Nyctaginaceae

The family Nyctaginaceae supplies 4 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

0 of 4 carry a published Janka test.

WoodJankaDensity
Black mampooGuapira fragrans960 lbf*38.0 lb/ft³
Corcho prietoGuapira obtusata1,054 lbf*39.6 lb/ft³
Umbrella catchbirdtreePisonia umbellifera276 lbf*21.2 lb/ft³
Water mampooPisonia subcordata395 lbf*25.1 lb/ft³