family
Nyssaceae
The family Nyssaceae supplies 5 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
2 of 5 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Black tupeloNyssa sylvatica | 810 lbf | 35.0 lb/ft³ |
| Dove treeDavidia involucrata | 791 lbf* | 34.7 lb/ft³ |
| Ogeechee tupeloNyssa ogeche | 791 lbf* | 34.7 lb/ft³ |
| Swamp tupeloNyssa biflora | 791 lbf* | 34.7 lb/ft³ |
| Water tupeloNyssa aquatica | 880 lbf | 35.0 lb/ft³ |