family
Olacaceae
The family Olacaceae supplies 4 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
1 of 4 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AfinaStrombosia glaucescens | 2,963 lbf* | 61.0 lb/ft³ |
| AngueukOngokea gore | 2,287 lbf* | 55.0 lb/ft³ |
| KulimScorodocarpus borneensis | 1,370 lbf | 54.0 lb/ft³ |
| Tallow woodXimenia americana | 1,923 lbf* | 52.4 lb/ft³ |