family
Oleaceae
The family Oleaceae supplies 28 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
5 of 28 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Berlandier ashFraxinus berlandieriana | 1,007 lbf* | 38.8 lb/ft³ |
| Black ashFraxinus nigra | 850 lbf | 34.3 lb/ft³ |
| Blue ashFraxinus quadrangulata | 1,107 lbf* | 40.6 lb/ft³ |
| BridgotreeChionanthus compactus | 4,196 lbf* | 75.4 lb/ft³ |
| Caca ravetForestiera rhamnifolia | 2,448 lbf* | 58.7 lb/ft³ |
| California privetLigustrum ovalifolium | 1,300 lbf* | 43.7 lb/ft³ |
| Carolina ashFraxinus caroliniana | 1,007 lbf* | 38.8 lb/ft³ |
| Caucasian ashFraxinus oxycarpa | 1,203 lbf* | 42.1 lb/ft³ |
| Chinese fringetreeChionanthus retusus | 1,923 lbf* | 52.4 lb/ft³ |
| Chinese privetLigustrum sinense | 1,852 lbf* | 51.5 lb/ft³ |
| Common lilacSyringa vulgaris | 2,064 lbf* | 54.2 lb/ft³ |
| East African OliveOlea hochstetteri | 2,740 lbf | 55.0 lb/ft³ |
| European ashFraxinus excelsior | 1,007 lbf* | 38.8 lb/ft³ |
| Glossy privetLigustrum lucidum | 1,203 lbf* | 42.1 lb/ft³ |
| Goodding's ashFraxinus gooddingii | 1,007 lbf* | 38.8 lb/ft³ |
| Green ashFraxinus pennsylvanica | 1,200 lbf | 39.1 lb/ft³ |
| Japanese privetLigustrum japonicum | 1,203 lbf* | 42.1 lb/ft³ |
| Japanese tree lilacSyringa reticulata | 1,103 lbf* | 40.5 lb/ft³ |
| Narrow-leafed ashFraxinus angustifolia | 1,007 lbf* | 38.8 lb/ft³ |
| OliveOlea europaea | 3,336 lbf* | 67.7 lb/ft³ |
| Oregon ashFraxinus latifolia | 1,160 lbf | 38.5 lb/ft³ |
| Palo de huesoHaenianthus salicifolius | 2,867 lbf* | 63.1 lb/ft³ |
| Pumpkin ashFraxinus profunda | 875 lbf* | 36.3 lb/ft³ |
| Shamel ashFraxinus uhdei | 1,203 lbf* | 42.1 lb/ft³ |
| Texas ashFraxinus texensis | 1,007 lbf* | 38.8 lb/ft³ |
| Velvet ashFraxinus velutina | 1,007 lbf* | 38.8 lb/ft³ |
| White ashFraxinus americana | 1,320 lbf | 42.0 lb/ft³ |
| White rosewoodChionanthus domingensis | 2,963 lbf* | 64.1 lb/ft³ |