The family Phyllanthaceae supplies 5 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

0 of 5 carry a published Janka test.

WoodJankaDensity
Antidesma buniusAntidesma bunius1,475 lbf*46.4 lb/ft³
Bastard hogberryMargaritaria nobilis1,852 lbf*51.5 lb/ft³
Ha aAntidesma platyphyllum1,923 lbf*52.4 lb/ft³
PoumuliFlueggea flexuosa2,064 lbf*54.2 lb/ft³
Tahitian gooseberry treePhyllanthus acidus1,255 lbf*43.0 lb/ft³