family
Piperaceae
The family Piperaceae supplies 5 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
0 of 5 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Guyanese pepperPiper glabrescens | 423 lbf* | 26.0 lb/ft³ |
| Higuillo de hoja menudaPiper aduncum | 573 lbf* | 29.8 lb/ft³ |
| Higuillo de limonPiper amalago | 1,152 lbf* | 41.3 lb/ft³ |
| Jamaican pepperPiper hispidum | 714 lbf* | 33.1 lb/ft³ |
| Moth pepperPiper blattarum | 714 lbf* | 33.1 lb/ft³ |