Wood Record

family

Platanaceae

The family Platanaceae supplies 6 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

1 of 6 carry a published Janka test.

WoodJankaDensity
American sycamorePlatanus occidentalis770 lbf34.3 lb/ft³
Arizona sycamorePlatanus wrightii791 lbf*34.7 lb/ft³
California sycamorePlatanus racemosa791 lbf*34.7 lb/ft³
London planetreePlatanus hybrida791 lbf*34.7 lb/ft³
Mexican sycamorePlatanus mexicana791 lbf*34.7 lb/ft³
Oriental planetreePlatanus orientalis791 lbf*34.7 lb/ft³