Wood Record

family

Podocarpaceae

The family Podocarpaceae supplies 9 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

4 of 9 carry a published Janka test.

WoodJankaDensity
East African yellowwoodAfrocarpus gracilior791 lbf*34.7 lb/ft³
Huon pineLagarostrobos franklinii926 lbf*43.0 lb/ft³
PodoPodocarpus spp.830 lbf32.0 lb/ft³
PodocarpPodocarpus spp.760 lbf35.0 lb/ft³
RimúDacrydium spp.785 lbf35.0 lb/ft³
TotaraPodocarpus spp.655 lbf32.0 lb/ft³
YellowwoodAfrocarpus falcatus714 lbf*33.1 lb/ft³
Yew plum pinePodocarpus macrophyllus898 lbf*42.1 lb/ft³
Yucca plum pinePodocarpus coriaceus1,255 lbf*43.0 lb/ft³