Wood Record

family

Primulaceae

The family Primulaceae supplies 8 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

0 of 8 carry a published Janka test.

WoodJankaDensity
Bois bandeJacquinia berteroi2,139 lbf*55.1 lb/ft³
BraceletwoodJacquinia armillaris1,598 lbf*48.1 lb/ft³
China-shrubArdisia solanacea1,152 lbf*41.3 lb/ft³
Guadeloupe marlberryArdisia obovata1,475 lbf*46.4 lb/ft³
Kokea lau liiMyrsine sandwicensis1,255 lbf*43.0 lb/ft³
Kolea lau nuiMyrsine lessertiana1,203 lbf*42.1 lb/ft³
Lanai colicwoodMyrsine lanaiensis1,538 lbf*47.3 lb/ft³
Leathery colicwoodMyrsine coriacea1,363 lbf*44.7 lb/ft³