Wood Record

family

Proteaceae

The family Proteaceae supplies 5 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

2 of 5 carry a published Janka test.

WoodJankaDensity
KahiliflowerGrevillea banksii1,255 lbf*43.0 lb/ft³
Louro-faiaRoupala montana2,169 lbf61.3 lb/ft³
Macadamia NutMacadamia tetraphylla1,538 lbf*47.3 lb/ft³
Macadamia nut tree, penguaMacadamia integrifolia2,064 lbf*54.2 lb/ft³
Silky-OakGrevillea robusta840 lbf38.0 lb/ft³