Wood Record

family

Putranjivaceae

The family Putranjivaceae supplies 2 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

0 of 2 carry a published Janka test.

WoodJankaDensity
Guiana plumDrypetes lateriflora2,287 lbf*56.9 lb/ft³
VaritalDrypetes glauca1,852 lbf*51.5 lb/ft³