The family Rhizophoraceae supplies 12 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

2 of 12 carry a published Janka test.

WoodJankaDensity
BiutCeriops tagal2,963 lbf*64.1 lb/ft³
GoatwoodCassipourea guianensis2,210 lbf*55.9 lb/ft³
MangleRhizophora apiculata3,965 lbf*73.4 lb/ft³
Mangle ColoradoRhizophora mangle2,760 lbf67.0 lb/ft³
Mangle hembraRhizophora mucronata2,607 lbf*60.4 lb/ft³
Oriental mangroveBruguiera gymnorhiza2,448 lbf*58.7 lb/ft³
Oriental mangroveBruguiera sexangula2,530 lbf*59.6 lb/ft³
OvogaPoga oleosa451 lbf*27.0 lb/ft³
PillarwoodCassipourea malosana1,450 lbf47.0 lb/ft³
Rhizophora stylosaRhizophora stylosa2,607 lbf*60.4 lb/ft³
SaitamuCrossostylis biflora1,007 lbf*38.8 lb/ft³
Smallflower bruguieraBruguiera parviflora2,692 lbf*61.3 lb/ft³