Wood Record

family

Rosaceae

The family Rosaceae supplies 55 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

2 of 55 carry a published Janka test.

WoodJankaDensity
Allegheny plumPrunus alleghaniensis832 lbf*35.5 lb/ft³
Allegheny serviceberryAmelanchier laevis1,852 lbf*51.5 lb/ft³
American mountain-ashSorbus americana1,103 lbf*40.5 lb/ft³
American plumPrunus americana832 lbf*35.5 lb/ft³
AppleMalus domestica1,658 lbf*48.9 lb/ft³
ApricotPrunus armeniaca1,725 lbf*49.9 lb/ft³
Bitter cherryPrunus emarginata832 lbf*35.5 lb/ft³
Black cherryPrunus serotina950 lbf35.0 lb/ft³
Bronze loquatEriobotrya deflexa2,692 lbf*61.3 lb/ft³
Callery pearPyrus calleryana1,255 lbf*43.0 lb/ft³
Canada plumPrunus nigra832 lbf*35.5 lb/ft³
Carolina laurelcherryPrunus caroliniana832 lbf*35.5 lb/ft³
Cherry laurelPrunus laurocerasus875 lbf*36.3 lb/ft³
Cherry plumPrunus cerasifera832 lbf*35.5 lb/ft³
Chickasaw plumPrunus angustifolia832 lbf*35.5 lb/ft³
Chinese pearPyrus pyrifolia1,255 lbf*43.0 lb/ft³
ChokecherryPrunus virginiana832 lbf*35.5 lb/ft³
Cockspur hawthornCrataegus crus-galli1,598 lbf*48.1 lb/ft³
Common pearPyrus communis1,255 lbf*43.0 lb/ft³
Common serviceberryAmelanchier arborea1,852 lbf*51.5 lb/ft³
Curlleaf mountain-mahoganyCercocarpus ledifolius2,448 lbf*58.7 lb/ft³
Downy hawthornCrataegus mollis1,852 lbf*51.5 lb/ft³
European mountain-ashSorbus aucuparia1,054 lbf*39.6 lb/ft³
European plumPrunus domestica832 lbf*35.5 lb/ft³
Greene's mountain ashSorbus scopulina1,054 lbf*39.6 lb/ft³
Japanese flowering cherryPrunus serrulata832 lbf*35.5 lb/ft³
Japanese flowering crab appleMalus floribunda1,538 lbf*47.3 lb/ft³
Japanese plumPrunus salicina832 lbf*35.5 lb/ft³
LoquatEriobotrya japonica2,448 lbf*58.7 lb/ft³
Mahaleb cherryPrunus mahaleb832 lbf*35.5 lb/ft³
Mexican plumPrunus mexicana832 lbf*35.5 lb/ft³
MueriPygeum africanum1,860 lbf45.0 lb/ft³
Northern mountain-ashSorbus decora1,054 lbf*39.6 lb/ft³
Oneseed hawthornCrataegus monogyna1,725 lbf*49.9 lb/ft³
Oregon crab appleMalus fusca1,538 lbf*47.3 lb/ft³
Paradise appleMalus pumila1,538 lbf*47.3 lb/ft³
PeachPrunus persica832 lbf*35.5 lb/ft³
Pear hawthornCrataegus calpodendron1,725 lbf*49.9 lb/ft³
Pin cherryPrunus pensylvanica832 lbf*35.5 lb/ft³
Prairie crab appleMalus ioensis1,538 lbf*47.3 lb/ft³
QuinceCydonia oblonga1,475 lbf*46.4 lb/ft³
Roundleaf serviceberryAmelanchier sanguinea1,852 lbf*51.5 lb/ft³
Sargent cherryPrunus sargentii832 lbf*35.5 lb/ft³
Scarlet hawthornCrataegus pedicellata1,788 lbf*50.7 lb/ft³
Siberian crab appleMalus baccata1,538 lbf*47.3 lb/ft³
Sour cherryPrunus cerasus832 lbf*35.5 lb/ft³
Southern crab appleMalus angustifolia1,538 lbf*47.3 lb/ft³
Sweet almondPrunus dulcis832 lbf*35.5 lb/ft³
Sweet crab appleMalus coronaria1,538 lbf*47.3 lb/ft³
ToyonHeteromeles arbutifolia1,923 lbf*52.4 lb/ft³
Washington hawthornCrataegus phaenopyrum1,658 lbf*48.9 lb/ft³
West Indian cherryPrunus myrtifolia1,923 lbf*52.4 lb/ft³
Western cherry laurelPrunus occidentalis2,287 lbf*56.9 lb/ft³
Western mountain ashSorbus sitchensis1,054 lbf*39.6 lb/ft³
Wild cherryPrunus avium1,152 lbf*41.3 lb/ft³