family
Rubiaceae
The family Rubiaceae supplies 39 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
6 of 39 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AburaMitragyna ciliata | 780 lbf | 34.0 lb/ft³ |
| AfaNeonauclea forsteri | 1,419 lbf* | 45.5 lb/ft³ |
| Aidia racemosaAidia racemosa | 2,367 lbf* | 57.7 lb/ft³ |
| AlaheePsydrax odorata | 2,448 lbf* | 58.7 lb/ft³ |
| Arabian coffeeCoffea arabica | 1,598 lbf* | 48.1 lb/ft³ |
| AraríbaSickingia spp. | 1,054 lbf* | 40.0 lb/ft³ |
| Cachimbo grandePsychotria grandis | 753 lbf* | 33.9 lb/ft³ |
| Caribbean princewoodExostema caribaeum | 3,336 lbf* | 67.7 lb/ft³ |
| Coffea libericaCoffea liberica | 2,139 lbf* | 55.1 lb/ft³ |
| Cucubano de monteGuettarda valenzuelana | 1,363 lbf* | 44.7 lb/ft³ |
| Cucubano de viequesGuettarda odorata | 2,139 lbf* | 55.1 lb/ft³ |
| DegameCalycophyllum candidissimum | 1,940 lbf | 51.0 lb/ft³ |
| False coffeeFaramea occidentalis | 1,538 lbf* | 47.3 lb/ft³ |
| FatporkChione venosa | 1,658 lbf* | 48.9 lb/ft³ |
| HalduAdina cordifolia | 1,140 lbf | 44.0 lb/ft³ |
| Hammock velvetseedGuettarda elliptica | 2,064 lbf* | 54.2 lb/ft³ |
| Indian mulberryMorinda citrifolia | 791 lbf* | 34.7 lb/ft³ |
| JaguaGenipa americana | 1,410 lbf | 44.0 lb/ft³ |
| KadamAnthocephalus chinensis | 600 lbf | 26.0 lb/ft³ |
| KadamNeolamarckia cadamba | 573 lbf* | 29.8 lb/ft³ |
| KopikoulaPsychotria hawaiiensis | 1,152 lbf* | 41.3 lb/ft³ |
| LiberalTimonius timon | 1,103 lbf* | 40.5 lb/ft³ |
| ManunuTarenna sambucina | 1,203 lbf* | 42.1 lb/ft³ |
| OlaCyclophyllum barbatum | 1,598 lbf* | 48.1 lb/ft³ |
| OlomeaAidia cochinchinensis | 2,530 lbf* | 59.6 lb/ft³ |
| OpepeNauclea diderrichii | 1,630 lbf | 47.0 lb/ft³ |
| OpikoPsychotria mauiensis | 1,419 lbf* | 45.5 lb/ft³ |
| Palicourea croceoidesPalicourea croceoides | 875 lbf* | 36.3 lb/ft³ |
| Palo de hierroIxora ferrea | 2,287 lbf* | 56.9 lb/ft³ |
| PuapuaGuettarda speciosa | 1,152 lbf* | 41.3 lb/ft³ |
| Pubescent mirrorplantCoprosma pubens | 1,255 lbf* | 43.0 lb/ft³ |
| QuinineCinchona pubescens | 1,103 lbf* | 40.5 lb/ft³ |
| Red cappelPalicourea crocea | 1,054 lbf* | 39.6 lb/ft³ |
| ScarletbushHamelia patens | 641 lbf* | 31.5 lb/ft³ |
| Showy cappelPalicourea guianensis | 753 lbf* | 33.9 lb/ft³ |
| Voa vangaVangueria madagascariensis | 1,203 lbf* | 42.1 lb/ft³ |
| White indigoberryRandia aculeata | 1,990 lbf* | 53.3 lb/ft³ |
| Wild guaveGuettarda scabra | 1,852 lbf* | 51.5 lb/ft³ |
| Woodland mirrorplantCoprosma rhynchocarpa | 1,475 lbf* | 46.4 lb/ft³ |