The family Rutaceae supplies 27 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

5 of 27 carry a published Janka test.

WoodJankaDensity
AceitilloPilocarpus racemosus3,647 lbf*70.6 lb/ft³
Amur corktreePhellodendron amurense679 lbf*32.3 lb/ft³
Citrus maximaCitrus maxima1,725 lbf*49.9 lb/ft³
Citrus medicaCitrus medica1,923 lbf*52.4 lb/ft³
Common hoptreePtelea trifoliata2,210 lbf*55.9 lb/ft³
Common pricklyashZanthoxylum americanum1,152 lbf*41.3 lb/ft³
Dotted pricklyashZanthoxylum punctatum2,963 lbf*64.1 lb/ft³
East African SatinwoodPagara macrophylla2,064 lbf*53.0 lb/ft³
East Indian SatinwoodChloroxylon swietenia2,600 lbf61.0 lb/ft³
Flower axistreeGlycosmis parviflora1,203 lbf*42.1 lb/ft³
Hercules' clubZanthoxylum clava-herculis1,203 lbf*42.1 lb/ft³
KukaemoaMelicope clusiifolia1,255 lbf*43.0 lb/ft³
LimeberryTriphasia trifolia915 lbf*37.1 lb/ft³
Limon chinaCitrus hystrix1,658 lbf*48.9 lb/ft³
MafuFagaropsis angolensis1,370 lbf43.0 lb/ft³
Maminha-de-porcaZanthoxylum rhoifolium = Zanthoxylum regnelianum791 lbf37.5 lb/ft³
Murraya koenigiiMurraya koenigii1,658 lbf*48.9 lb/ft³
Pau marfimBalfourodendron riedelianum2,367 lbf*57.7 lb/ft³
Pau-amareloEuxylophora paraensis2,168 lbf50.6 lb/ft³
Prickly yellowZanthoxylum caribaeum1,923 lbf*52.4 lb/ft³
Queensland mapleFlindersia brayleyana915 lbf*37.1 lb/ft³
Queensland-MapleFlindersia spp.725 lbf35.0 lb/ft³
Sea torchwoodAmyris elemifera3,749 lbf*71.5 lb/ft³
SoopiniMelicope latifolia753 lbf*33.9 lb/ft³
TalafuluMicromelum minutum1,990 lbf*53.3 lb/ft³
West Indian satinwoodZanthoxylum flavum2,448 lbf*58.7 lb/ft³
White pricklyashZanthoxylum martinicense832 lbf*35.5 lb/ft³