3 of 42 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Arroyo willowSalix lasiolepis | 791 lbf* | 34.7 lb/ft³ |
| Balsam poplarPopulus balsamifera | 351 lbf* | 23.8 lb/ft³ |
| Balsam willowSalix pyrifolia | 451 lbf* | 26.7 lb/ft³ |
| Batoko plumFlacourtia inermis | 2,367 lbf* | 57.7 lb/ft³ |
| Bebb willowSalix bebbiana | 451 lbf* | 26.7 lb/ft³ |
| Bigtooth aspenPopulus grandidentata | 471 lbf* | 27.3 lb/ft³ |
| Black cottonwoodPopulus balsamifera ssp. trichocarpa | 350 lbf | 24.5 lb/ft³ |
| Black poplarPopulus nigra | 509 lbf* | 28.2 lb/ft³ |
| Black willowSalix nigra | 471 lbf* | 27.3 lb/ft³ |
| Bonpland willowSalix bonplandiana | 451 lbf* | 26.7 lb/ft³ |
| Coastal plain willowSalix caroliniana | 451 lbf* | 26.7 lb/ft³ |
| Corkscrew willowSalix matsudana | 451 lbf* | 26.7 lb/ft³ |
| Crack willowSalix fragilis | 451 lbf* | 26.7 lb/ft³ |
| CrackopenCasearia sylvestris | 1,598 lbf* | 48.1 lb/ft³ |
| Dense logwoodXylosma congestum | 1,437 lbf* | 45.8 lb/ft³ |
| Diamondleaf willowSalix planifolia | 451 lbf* | 26.7 lb/ft³ |
| Eastern cottonwoodPopulus deltoides | 430 lbf | 28.0 lb/ft³ |
| Elaeagnus willowSalix elaeagnos | 451 lbf* | 26.7 lb/ft³ |
| FilimotoFlacourtia rukam | 2,530 lbf* | 59.6 lb/ft³ |
| Fremont cottonwoodPopulus fremontii | 608 lbf* | 30.7 lb/ft³ |
| Geyer willowSalix geyeriana | 451 lbf* | 26.7 lb/ft³ |
| Gia verdeCasearia arborea | 1,475 lbf* | 46.4 lb/ft³ |
| Goodding's willowSalix gooddingii | 451 lbf* | 26.7 lb/ft³ |
| Governor's plumFlacourtia indica | 1,852 lbf* | 51.5 lb/ft³ |
| GuasimillaProckia crucis | 1,598 lbf* | 48.1 lb/ft³ |
| Guyanese wild coffeeCasearia guianensis | 1,990 lbf* | 53.3 lb/ft³ |
| Narrowleaf cottonwoodPopulus angustifolia | 423 lbf* | 26.0 lb/ft³ |
| Peachleaf willowSalix amygdaloides | 451 lbf* | 26.7 lb/ft³ |
| Pussy willowSalix discolor | 451 lbf* | 26.7 lb/ft³ |
| Quaking aspenPopulus tremuloides | 350 lbf | 26.6 lb/ft³ |
| Rabo de rantonCasearia aculeata | 1,725 lbf* | 49.9 lb/ft³ |
| Red willowSalix laevigata | 451 lbf* | 26.7 lb/ft³ |
| Salix humboldtianaSalix humboldtiana | 573 lbf* | 29.8 lb/ft³ |
| Scouler's willowSalix scouleriana | 451 lbf* | 26.7 lb/ft³ |
| Silky willowSalix sericea | 451 lbf* | 26.7 lb/ft³ |
| Silver poplarPopulus alba | 423 lbf* | 26.0 lb/ft³ |
| Sitka willowSalix sitchensis | 451 lbf* | 26.7 lb/ft³ |
| Swamp cottonwoodPopulus heterophylla | 423 lbf* | 26.0 lb/ft³ |
| White cogwoodHomalium racemosum | 2,210 lbf* | 55.9 lb/ft³ |
| White willowSalix alba | 451 lbf* | 26.7 lb/ft³ |
| Wild honeytreeCasearia decandra | 1,788 lbf* | 50.7 lb/ft³ |
| Yellow willowSalix lutea | 451 lbf* | 26.7 lb/ft³ |