Santalaceae
The family Santalaceae supplies 2 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
1 of 2 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Mountain sandalwoodSantalum paniculatum | 1,852 lbf* | 51.5 lb/ft³ |
| SandalwoodSantalum album | 1,680 lbf | 58.0 lb/ft³ |