family
Simaroubaceae
The family Simaroubaceae supplies 6 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
1 of 6 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Aceitillo falsoSimarouba tulae | 1,309 lbf* | 43.8 lb/ft³ |
| AilanthusAilanthus altissima | 791 lbf* | 34.7 lb/ft³ |
| BitterwoodPicrasma excelsa | 608 lbf* | 30.7 lb/ft³ |
| MarupáSimarouba amara | 452 lbf | 27.5 lb/ft³ |
| OnzangOdyendea spp. | 344 lbf* | 24.0 lb/ft³ |
| ParadisetreeSimarouba glauca | 608 lbf* | 30.7 lb/ft³ |