Wood Record

family

Solanaceae

The family Solanaceae supplies 6 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

0 of 6 carry a published Janka test.

WoodJankaDensity
Earleaf nightshadeSolanum mauritianum573 lbf*29.8 lb/ft³
Forest nightshadeSolanum nudum753 lbf*33.9 lb/ft³
Mullein nightshadeSolanum donianum542 lbf*29.1 lb/ft³
PotatotreeSolanum erianthum679 lbf*32.3 lb/ft³
Tree tobaccoNicotiana glauca641 lbf*31.5 lb/ft³
Turkey berrySolanum torvum542 lbf*29.1 lb/ft³