family
Sterculiaceae
The family Sterculiaceae supplies 12 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
12 of 12 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| AxixáSterculia apeibophylla | 686 lbf | 38.1 lb/ft³ |
| Brown SterculiaSterculia rhinopetala | 1,810 lbf | 50.0 lb/ft³ |
| ChichaSterculia apetala | 400 lbf | 25.0 lb/ft³ |
| DantaNesogordonia papaverifera | 2,140 lbf | 50.0 lb/ft³ |
| Fava-brancaStryphnodendron pulcherrimum | 1,310 lbf | 38.1 lb/ft³ |
| MansoniaMansonia altissima | 1,290 lbf | 42.0 lb/ft³ |
| MengkulangHeritiera spp. | 1,230 lbf | 42.0 lb/ft³ |
| NiangonTarrietia utilis | 1,100 lbf | 41.3 lb/ft³ |
| ObecheTriplochiton scleroxylon | 430 lbf | 24.0 lb/ft³ |
| PterygotaPterygota spp. | 955 lbf | 39.0 lb/ft³ |
| SterculiaSterculia pruriens | 798 lbf | 37.0 lb/ft³ |
| Yellow SterculiaSterculia oblonga | 1,120 lbf | 48.0 lb/ft³ |