family
Styracaceae
The family Styracaceae supplies 5 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
0 of 5 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| Carolina silverbellHalesia carolina | 641 lbf* | 31.5 lb/ft³ |
| Japanese snowbellStyrax japonicus | 1,054 lbf* | 39.6 lb/ft³ |
| Little silverbellHalesia parviflora | 641 lbf* | 31.5 lb/ft³ |
| Mountain silverbellHalesia tetraptera | 641 lbf* | 31.5 lb/ft³ |
| Two-wing silverbellHalesia diptera | 641 lbf* | 31.5 lb/ft³ |