Wood Record

family

Tamaricaceae

The family Tamaricaceae supplies 3 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

0 of 3 carry a published Janka test.

WoodJankaDensity
Athel tamariskTamarix aphylla1,255 lbf*43.0 lb/ft³
Five-stamen tamariskTamarix chinensis1,054 lbf*39.6 lb/ft³
SaltcedarTamarix ramosissima1,788 lbf*50.7 lb/ft³