The family Taxaceae supplies 6 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.
0 of 6 carry a published Janka test.
| Wood | Janka | Density |
|---|---|---|
| California torreya (nutmeg)Torreya californica | 599 lbf* | 32.3 lb/ft³ |
| European yewTaxus baccata | 1,009 lbf* | 45.5 lb/ft³ |
| Florida torreya (nutmeg)Torreya taxifolia | 645 lbf* | 33.9 lb/ft³ |
| Florida yewTaxus floridana | 1,038 lbf* | 46.4 lb/ft³ |
| Japanese yewTaxus cuspidata | 1,038 lbf* | 46.4 lb/ft³ |
| Pacific yewTaxus brevifolia | 1,038 lbf* | 46.4 lb/ft³ |