Wood Record

family

Theaceae

The family Theaceae supplies 5 of the timbers in this database. A family shares broad anatomy, but not necessarily working properties.

1 of 5 carry a published Janka test.

WoodJankaDensity
CamelliaCamellia japonica1,725 lbf*49.9 lb/ft³
Deciduous StewartiaStewartia pseudocamellia1,658 lbf*48.9 lb/ft³
Loblolly-bayGordonia lasianthus679 lbf*32.3 lb/ft³
NeedlewoodSchlma spp.1,245 lbf43.0 lb/ft³
TeaCamellia sinensis915 lbf*37.1 lb/ft³